Sun. Nov 28th, 2021

Special soft cracking slurry operation process
Instructions

  1. The screen is 80-100 mesh, and the screen is printed with a hard square knife at 75 degrees. First, use the cracked transparent paste to make the bottom printing 1-2 times, and the first board is hard to scrape 4-6 knives
  2. Stir the cracked white glue, transparent paste, color paste and curing agent evenly and print 2-3 times (3-4 times each time)
  3. Spontaneous combustion, drying and bursting
  4. Raising the cloth
    [Characteristics for use] This product has a natural cracking-like effect after printing and drying
    [Composition] It is composed of cracked white pulp, cracked transparent pulp and transparent base
    [Process] Transparent printing and printing → cracked pulp → blow-drying or natural drying and bursting → cloth picking → pressing and overheating → finished product
    [Note] 1. If the glue paste is too thick before printing, add water, do not reinforce the paste so as not to affect the bursting effect.
    【Application Reference】
    Note: It is recommended that the cracked paste is exposed to thick screen printing, and it is best to print enough color at a time. If you use thin screen printing, please use cold air to blow the surface of the paste layer, and reprint before the paste layer cracks. (The size of the crack is related to How much can be controlled by the matching ratio of crack white and crack transparency and the thickness of the printed slurry layer. The more the crack transparency ratio and the thinner the printed slurry layer, the finer the cracks, and the thicker the cracks. .Special emphasis: the moire pulp must be equipped with a transparent primer, otherwise it is easy to fall off and has no elasticity. The above process is for reference only, and the factory can adjust it according to the actual situation.

Leave a Reply